• ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
  • ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard
ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard

ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard

Dettagli:

Luogo di origine: Hunan, Cina

Termini di pagamento e spedizione:

Quantità di ordine minimo: 100
Prezzo: $9-20
Miglior prezzo Contatto

Informazioni dettagliate

Composizione chimica: Al Materiale: Alluminio
Contenuto di Al: Leghe di alluminio Tipo in lega: Leghe di Al-Zn-In
Contenuto dello Zn: 2,5-7,0% Nel contenuto: 0,018-0,050%
Contenuto del CD: 0,005-0,020% Contenuto Sn: 0,018-0,075%
Contenuto di mg: 0,50-1,50% Contenuto di si: 0,10-0,15%
Contenuto del Ti: 0.01-0.08% Tensione a circuito aperto: da -1,18 a -1,10 V
Tensione di circuito chiuso: da -1,12 a -1,05 V Capacità effettiva: ≥2400Ah/kg
Efficienza attuale: ≥85%
Evidenziare:

ISO9001:2008 Certified Sacrificial Aluminum Anode

,

GB/T 4948-2002 Standard Aluminum Bracelet Anode

,

Galvanic Corrosion Protection Aluminum Alloy Anode

Descrizione di prodotto

Sacrificial Aluminum Bracelet Anodes for Galvanic Corrosion
Sacrificial bracelet anodes are typically made from either zinc alloy or aluminum alloy, depending on design requirements, environmental variables, and water salinity. These anodes provide cost-effective and reliable cathodic protection for submerged pipelines, which are usually coated with anti-corrosion materials and weighted with concrete for negative buoyancy.
Bracelet anodes are mounted at specific locations determined by the cathodic protection system design and are electrically connected to the pipeline via special bonding copper cables. While the primary defense against corrosion is the pipeline's anti-corrosion coating, bracelet anodes protect areas where coating failures may occur during installation or operation.
Sacrificial Aluminum Bracelet Anodes mounted on pipeline Close-up view of Sacrificial Aluminum Bracelet Anodes
Applications
These anodes are used for:
  • Hull protection
  • Ballast tanks
  • Offshore engineering
  • Harbor structures
  • Sea water cooling systems
  • Submerged pipelines
Chemical Composition Standards
Type Zn In Cd Sn Mg Si Ti Impurity (less than) Al
Al-Zn-In-Cd A11 2.5-4.5 0.018-0.050 0.005-0.020 - - -- - 0.10 Balance
Al-Zn-In-Sn A12 2.2-5.2 0.020-0.045 - 0.018-0.035 - - - 0.10 Balance
Al-Zn-In-Si A13 5.5-7.0 0.025-0.035 - - - 0.10-0.15 - 0.10 Balance
Al-Zn-In-Sn-Mg A14 2.5-4.0 0.020-0.050 - 0.025-0.075 0.50-1.00 - - 0.10 Balance
Al-Zn-In-Mg-Ti A21 4.0-7.0 0.02-0.050 - - 0.50-1.50 - 0.01-0.08 0.10 Balance
Electrochemical Characteristics
Item Material of anodes Open-circuit Voltage (v) Close-circuit Voltage (v) Actual Capacity(Ah/kg) Current efficiency (%) Consumption rate (kg.(A.a)) Dissolve Performance
Electrochemical Performance Type 1 -1.18- -1.10 -1.12- -1.05 ≥ 2400 ≥ 85 ≤ 3.65 The surface dissolve evenly & oxide drop easily
Type 2 -1.18- -1.10 -1.12- -1.05 ≥ 2600 ≥ 90 ≤ 3.37
Reference electrode: Saturated calomel electrode
Type 1: A11, A12, A13, A14
Type 2: A21
Why Choose Us?
Q. Why choose us?

A. We have over 20 years of experience in the cathodic protection anode market. Our products are strictly produced and tested according to American standard ASTM G97, ensuring continuous and stable high quality that saves you costs.

B. We offer prompt shipment. For urgent needs, we maintain stock of regular shape anodes to enable quick delivery, even when standard plant delivery time is 20 days.

Our sales office Our manufacturing workshop
Company Culture
  • Our Belief: Continuous Innovation
  • Our Spirit: Sincerity, Unity, Dedicated, Hardworking
  • Our Mission: Provide most advanced products & most professional technical solution
Certification
Our product certifications
Inspection & Lab
Our inspection and laboratory facilities

Vuoi conoscere maggiori dettagli su questo prodotto
Sono interessato a ISO9001:2008 Certified Sacrificial Aluminum Bracelet Anode for Galvanic Corrosion Protection with GB/T 4948-2002 Standard potresti inviarmi maggiori dettagli come tipo, dimensione, quantità, materiale, ecc.
Grazie!
Aspettando la tua risposta.